An Experimental Approach for Utilizing Waste Tea and Marble Dust in Concrete Blocks

Authors

  • DivyarajSinh Solanki School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Neel Suryawanshi School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Sweeti Sawant School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Shivam Bhise School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Parth Dabhole School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Prabhav Vakharia School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Shantini A. Bokil School of Civil Engineering, Dr. Vishwanath Karad MIT World Peace University, Pune-411038, India
  • Niraj S. Topare a:1:{s:5:"en_US";s:120:"Department Chemical Engineering, Bharati Vidyapeeth (Deemed to be University) College of Engineering, Pune 411043, India";}

Keywords:

PWTA, Marble Dust, Concrete, Sustainable, Tea

Abstract

Waste utilization has become vital in today's world which can help reduce toxicity levels. Waste can be recycled and reused in an effective way. Humans depend on natural resources and we extract around 60 million tons of natural resources each year for producing goods and services. Only 50% of the extracted resource is used in an efficient manner whereas 20 - 30% of natural resource is left over as waste. Incorporation of such waste into esteemed and emerging industries to attain sustainable, durable, and enduring products should be the aim of mankind today. The acronym PWTA stands for processed waste tea ash which is one such waste material that could be found in abundance around us. The PWTA can be used as a binder in the cementitious matrix used to make the concrete blocks. The mix design incorporated for casting the cubes included 7kg of ordinary portland cement of grade 53, 14kg of aggregate, 5kg fine aggregate (crushed sand), 2kg of Marble dust, and 300 grams of tea. The cementitious matrix was then poured into a cube of size 15cm x 15cm x 15cm. The 7th day of testing showed a value of 13.93 MPa, while we achieved 28 MPa on the 21st day of testing.

Vol. 1 No. 1 January 2024

Downloads

Published

2026-10-24

Issue

Section

Articles